汽车零件冲压工艺标识分类 1引言
·冲模技术·
汽车零件冲压工艺标识分类
张彦,张宗乐
长城汽车股份有限公司技术中心,河北省汽车工程技术研究中心(河北保定071000)
【摘要]随着当前生活水平的逐渐提高,人们对汽车的需求量越来越大,然而对汽车的品质要求也越来越高。主机厂在提高汽车品质方面,冲压工艺的完美是不可缺少的一部分,冲压工艺师往往通过一些方法来保证冲压工艺的完美性,如在冲压拉伸过程中使用到底标记;为保证装配的正确性,冲压件增加左右件标记;为达到钣金件的追溯,使用批次标识
等,本文中将重点介绍冲压工艺标识分类。关键词:到底标记;左右件标记;批次标识
中图分类号:TG385.2
文献标识码:B
IdentificationClassificationof Stamping
ProcessfortheAutomobileParts
[Abstract] With the gradual increase in the standard of living, people demand more and more on cars, however, are increasingly high requirements on automobile quality. Host plant in improving quality car is convenient, the stamping process of the perfect is an indispensable part of, stamping process engineeroften through some methods to ensurethe stamping process of the perfect, as in stamping drawing process in use in the end mark; prevent assembling is correct, stamping parts increase the left and right parts mark; retrospectively as the reach of sheet metal parts using batch identification, this paper will focus on the classification for stamping process identification
Key words: in the end mark; the left and right parts mark; batch mark
想做好冲压拉伸工艺,到底标识是不可忽视的。要想
要想做好汽车冲压工艺,细节是不容忽视的。要(3)后续工序制出安装销钉的平台,压料板一次
尽量直接铸出销钉,避让结构。
(4)不能设在双动侧冲活动滑块的凸模型面上。(5)拉伸凸模的CH孔位置,不能有立筋,不得已
的情况下,在CH孔位置设立筋的情况下应设置漏废料用空刀
(6)填堵拉伸模具的CH孔作业标准。填堵CH 孔的原因:成形时冲CH孔,使工序件发生变形,所以要填堵CH孔,要求填堵采用螺塞标准件,与模具材料相同。
《模具制造》2016年第8期万方数据
做到钣金件的可追溯性,批次标识是不可忽视的。 9结束语
CH孔作为整个模具加工制造及调试的定位系统,是提升冲压件精度提升的一个因素,所以在模具行业是不容忽视的。要求在模具验收过程中,也需要把CH孔作为一个重点项目来验收。
参考文献
[1]卢宁.浅谈CH孔应用技术[]模具制造,2015,(9)
第一作者简介:赵金升,男,1985年生,从事工作:汽车冲压制件开发。
(收稿日期:2016-03-11)owm
·33·