昆钢棒材连轧生产线工艺及设备特点
骆艳萍
(中冶南方工程技术有限公司,湖北武汉430223)
摘要:介绍昆钢新区棒材连轧生产线的生产工艺及平面布置.着重介绍了该生产线采用的热送热装、无孔型轧制、切分轧制、控制轧制及控制冷却工艺等多项节能新工艺和新技术,新工艺的应用降低了生产成本,提升了市场
竞争力,为昆钢带来了良好的经济效益,关键词:棒材轧制;工艺;设备
中图分类号:TG335
文献标识码:B
CharacteristicsofTechnologyandEquipmentoftheContinuousBar
RollingLineinKunmingIronandSteelCompany
LUO Yan ping
( WISDRI Engineering & Research Incorporation Limited, Wuhan,430223, P. R. China)
Abstract: The production technology and the plane layout of the continuous bar rolling line in Kunming Iron and Steel Company are introduced, the line uses a number of new energy saving technologies. It mainly introduces the hot delivery and hot charging, grooveless rolling, splitting rolling, controlled rolling and eontrolled cooling processes, these processes can reduce the production cost, enhance the market competitiveness, and bring good economic benefits for the company. Key words : bar rolling: process; equipment
0前言
武钢(集团)昆明钢铁股份有限公司(以下简称“昆钢”)为落实国家调整和振兴规划,在昆钢新区新建一条高性能抗震钢棒材连轧生产线.本工程采用先进、可靠、成熟的工艺设备和技术,确保产品质量和产量达到国内先进水平,为节省工程投资,生产线工艺设备全部由国内设计及制造,部分关键的配套件采用进口品牌.该生产线由中冶南方工程技术有限公司负责工艺技术、非标设计及工厂设计,自动化控制由中冶京城技术有限公司负责设计,加热炉由中冶南方威仕工业炉以EPC方式建设
生产工艺和设备特点
1
1.1轧线生产工艺
生产线设计产能为80万Va,Φ12mm带肋钢筋采用四切分工艺,Φ14mm带肋钢筋采用三切分工艺.Φ16~Φ20mm带肋钢筋采用两切分工艺生产.生产Φ40mm以下棒材时,1H~8V采用无孔型
收稿日期:2014-12-25
轧制,生产40mm以上棒材时,1H~2V采用无孔型轧制,其余主要采用椭圆-圆孔型系统,设计指标见表1.
棒材生产线设计指标
表1
项目
坏料规格/mm 产品规格/mm
加热炉能力/t·h-1 轧机数量/架
最高终轧速度/m·s-1
主要钢种定尺长度/m
设计指标
165 × 165 × 12 000
Φ12~Φ40(螺纹钢筋);
16~60(闽钢) 180(冷装额定产量)
18 18
抗震钢(HRB400(E)、 HRB500(E))、碳素结构钢(Q195、Q235)、优质碳素结构钢(45)、冷锻钢(ML40)、
合金结构钢(40Cr) 6~12
主广房内轧机采用高架式布置,轧线主要设备设置在+5.00m平台上,轧制中心线标高+5.80
作者简介:貉艳萍(1983-),女,2009年东北大学材料加工工程专业硕士研究生毕业,工程师,